Foshan Ruiang Technology Co., Ltd.
Foshan Chancheng District Ruijin Mould Factory
grades | WX-4 | WX-5 | WX-6 | WX-7 | WX-8 | 红-5 | 红-7 | 红-8 |
bulk density g/cm3 |
1.75 | 1.85 | 1.90 | 1.82 | 1.90 | 1.68 | 1.85 | 1.90 |
resistivity μΩm |
8-11 | 8-10 | 8-9 | 11~13 | 11-13 | 13-15 | 11-13 | 11~13 |
Thermal conductivity (100°C) W/m.k |
110-120 | 130-140 | 130-140 | 110-120 | 110-120 | 80-100 | 100-120 | 110-120 |
Coefficient of thermal expansion (room temperature - 600°C) 10-6/C |
5.46 | 4.75 | 4.8 | 5.8 | 5.85 | 5.8 | 5.9 | 5.85 |
Shore hardness HSD |
42 | 48 | 53 | 65 | 70 | 60 | 68 | 72 |
flexural strength Mpa |
38 | 46 | 55 | 51 | 60 | 38 | 62 | 70 |
compressive strength Mpa |
65 | 85 | 95 | 115 | 135 | 80 | 135 | 160 |
modulus of elasticity Gpa |
9 | 11.8 | 12 | 12 | 13 | 8.8 | 12 | 13 |
porosity % |
17 | 13 | 11 | 12 | 11 | 18 | 12 | 11 |
ash PPM |
500 | 500 | 500 | 500 | 500 | 500 | 500 | 500 |
Ash purification PPM |
50 | 50 | 50 | 50 | 50 | 50 | 50 | 50 |
granularity μm |
13-15 | 13-15 | 8-10 | 8-10 | 8-10 | 8-10 | 7 | 5 |
Recommended Applications | common (use) | common (use) |
continuous casting (metallurgy) Sintering Pyrometallurgy |
electric spark photovoltaic |
electric spark Photovoltaic Glass |
electric spark |
common (use) electric spark |
electric spark Photovoltaic Glass |
Isostatic graphite
Performance indicators of isostatic graphite materials for new energy vehicles and continuous casting industries.
grades | bulk density | resistivity | thermal conductivity |
Coefficient of thermal expansion (room temperature - 600°C) |
Shore hardness | flexural strength | compressive strength | modulus of elasticity | ash | Ash purification |
g/cm3 | μΩm | W/m.k | 10-6/℃ | HSD | Mpa | Mpa | Gpa | PPM | PPM | |
KYX-5 | 1.80 | 8-10 | 125 | 4.9 | 45 | 40 | 80 | 9.5 | 500 | 50 |
Isostatic graphite
Performance indicators of isostatic graphite materials for high temperature casting and ammonia fuel cell bipolar plate industry.
grades | bulk density | resistivity | thermal conductivity |
Coefficient of thermal expansion (room temperature - 600°C) |
Shore hardness | flexural strength | compressive strength | modulus of elasticity | ash | Ash purification |
g/cm3 | μΩm | W/m.k | 10-6/℃ | HSD | Mpa | Mpa | Gpa | PPM | PPM | |
KYX-5P | 1.90 | 8-10 | 135 | 4.0 | 55 | 55 | 105 | 12 | 500 | 50 |
Isostatic graphite
Performance indicators of isostatic graphite materials for semiconductor industry and 3D hot bending glass.
grades | bulk density | resistivity | thermal conductivity |
Coefficient of thermal expansion (room temperature - 600°C) |
Shore hardness | flexural strength | compressive strength | modulus of elasticity | Average particle size | |
g/cm3 | μΩm | W/m.k | 10-6/℃ | HSD | Mpa | Mpa | Gpa | μm | ||
KYD-8 | 1.84 | 10~14 | 125 | 4.2 | 50 | 50 | 115 | 11 | 5 |
Isostatic graphite
Performance index of isostatic graphite material for photovoltaic industry.
grades | bulk density | resistivity | thermal conductivity |
Coefficient of thermal expansion (room temperature - 600°C) |
Shore hardness | flexural strength | compressive strength | modulus of elasticity | ash | Ash purification |
g/cm3 | μΩm | W/m.k | 10-6/℃ | HSD | Mpa | Mpa | Gpa | PPM | PPM | |
KYD-4 | 1.72 | 10~13 | 100 | 5 | 40 | 30 | 65 | 9.2 | 500 | 50 |
KYD-6 | 1.81 | 11~14 | 120 | 4.5 | 60 | 45 | 90 | 10.5 | 500 | 50 |
Isostatic graphite
Performance index of isostatic graphite material for EDM industry.
grades | bulk density | resistivity | Shore hardness | Rockwell hardness | flexural strength | Average particle size |
g/cm3 | μΩm | HSD | HRL | Mpa | μm | |
KYX-7 | 1.76 | 12~16 | 40 | 94 | 40 | 8 |
KYX-60 | 1.78 | 12~16 | 45 | 100 | 45 | 4 |
Isostatic graphite
Performance index of isostatic graphite materials for other industries.
grades | bulk density | resistivity | thermal conductivity |
Coefficient of thermal expansion (room temperature - 600°C) |
Shore hardness | flexural strength | compressive strength | modulus of elasticity | Average particle size | |
g/cm3 | μΩm | W/m.k | 10-6/℃ | HSD | Mpa | Mpa | Gpa | μm | ||
KYD-30 | 1.81 | 15~19 | 80 | 5.8 | 80 | 43 | 130 | 7.5 | 12 | |
KYX-70 | 1.85 | 12~16 | 105 | 4.7 | 55 | 50 | 105 | 10 | 8 | |
KYX-60S | 1.88 | 12~16 | 110 | 4.5 | 60 | 55 | 120 | 11 | 4 | |
KYD-9 | 1.88-1.92 | 10~14 | 110 | 3.9 | 15 | 60 | 125 | 12 | 2 |
Reference table of physical and chemical indexes for different grades of isostatic moulding products | ||||||||||||||
Moulded Products:★Best Selling Products | ||||||||||||||
grades | bulk density | granularity | resistivity | thermal conductivity |
Coefficient of thermal expansion (room temperature - 600°C) |
Shore hardness | flexural strength | compressive strength | modulus of elasticity | porosity | ash | Ash purification | Main areas of application | |
g/cm3 | μm | μΩm | W/m.k | 10-6/℃ | HSD | Mpa | Mpa | Gpa | % | PPM | PPM | |||
KYM-2 | 1.50 | 11~13 | 12~15 | 80 | 6.2 | 30 | 15 | 32 | 6 | 22 | 500 | 50 | Graphite bearing granules, rotors, wipers | |
KYM-2 | 1.68 | 11~13 | 9~13 | 95 | 5.7 | 35 | 20 | 45 | 8 | 18 | 500 | 50 | Furniture and general yard crucibles | |
★KYM-5 | 1.80 | 11~13 | 8~10 | 125 | 4.9 | 48 | 35 | 70 | 9.5 | 13 | 500 | 50 |
sintering electric spark |
|
13~16 |
Pre-pressure products:★Best-selling products | ||||||||||||||
grades | bulk density | granularity | resistivity | thermal conductivity |
Coefficient of thermal expansion (room temperature - 600°C) |
Shore hardness | flexural strength | compressive strength | modulus of elasticity | porosity | ash | Ash purification | Main areas of application | |
g/cm3 | μm | μΩm | W/m.k | 10-6/℃ | HSD | Mpa | Mpa | Gpa | % | PPM | PPM | |||
★KY-7 | 1.76 | 8~10 | 12~16 | 90 | 5.2 | 40 | 35 | 60 | 9 | 18 | 500 | 50 | electric spark, special purpose graphite | |
KY-70 | 1.80 | 2~4 | 12~16 | 95 | 4.7 | 45 | 40 | 80 | 10 | 12 | 500 | 50 | ||
KY-70S | 1.85 | 2~4 | 12~16 | 100 | 4.2 | 55 | 50 | 105 | 11 | 11 | 500 | 50 |
Isostatic Pressure Products:★Best Selling Products | ||||||||||||||
grades | bulk density | granularity | resistivity | thermal conductivity |
Coefficient of thermal expansion (room temperature - 600°C) |
Shore hardness | flexural strength | compressive strength | modulus of elasticity | porosity | ash | Ash purification | Main areas of application | |
g/cm3 | μm | μΩm | W/m.k | 10-6/℃ | HSD | Mpa | Mpa | Gpa | % | PPM | PPM | |||
KYD-4 | 1.72 | 25 | 10~13 | 100 | 5 | 40 | 30 | 65 | 9.2 | 17 | 500 | 50 | Vacuum furnace, sintering | |
★KYD-6 | 1.81 | 11~13 | 11~14 | 120 | 4.5 | 60 | 45 | 90 | 10.5 | 12 | 500 | 50 | Photovoltaic, vacuum furnace | |
KYD-8 | 1.84 | 6 | 10~14 | 110 | 4 | 72 | 55 | 120 | 12 | 12 | 500 | 50 | electric spark, gold melting crucibles | |
★KYD-9 | 1.88~1.92 | 2-4 | 10~14 | 110 | 3.9 | 75 | 60 | 125 | 12 | 10 | 500 | 50 | electric spark, gold melting crucibles | |
KYD-30 | 1.81 | 11~13 | 15~19 | 80 | 5.8 | 80 | 43 | 130 | 7.5 | 12 | 500 | 50 | electric spark, super hard graphite |
Note:1.Product performance is the index of product centre position; 2.Porosity is the sum of open and closed porosity; 3.The above values are representative characteristics, not guaranteed values;